Stir SpA SR 70 (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Stir SpA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA SR 70 (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Extrusion sheath with good flexibility type TM-2Cold flex = -33°CInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.422 g/cc
0.05137 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength at Break 13.5 MPa
1960 psi
ISO R 527
Elongation at Break 360 %
360 %
ISO R 527