Stir SpA LG 57 AT 1 (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Stir SpA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA LG 57 AT 1 (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Extrusion for ecological cordsInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
ISO 868
Tensile Strength at Break 8.51 MPa
1230 psi
ISO R 527
Elongation at Break 387 %
387 %
ISO R 527