Stir SpA AF 80 3 GEC (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Stir SpA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA AF 80 3 GEC (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Insulation CEI 20-11 type TI 1 low acid fumes emissionInformation provided by STIR SpA
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ISO 868
Tensile Strength at Break 15.2 MPa
2200 psi
ISO R 527
Elongation at Break 202 %
202 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 30.2 %
30.2 %
ASTM D2863