Special Metals Nickel 212

Category Metal , Nonferrous Metal , Nickel Alloy , Pure Element
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals Nickel 212.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wrought nickel strengthened with an added manganese. Used for electrical and electronic applications such as lead wires, supporting components in lamps and cathode-ray tubes, and electrodes in glow-discharge lamps. The standard product form is wire.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Thermal Properties Metric English Comments
CTE, linear 12.9 µm/m-°C

@Temperature 20.0 - 100 °C
7.17 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.430 J/g-°C
0.103 BTU/lb-°F
Thermal Conductivity 44.0 W/m-K
305 BTU-in/hr-ft²-°F
Melting Point 1435 - 1446 °C
2615 - 2635 °F
Solidus 1435 °C
2615 °F
Liquidus 1446 °C
2635 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Copper, Cu <= 0.20 %
<= 0.20 %
Iron, Fe <= 0.25 %
<= 0.25 %
Magnesium, Mg <= 0.20 %
<= 0.20 %
Manganese, Mn 1.5 - 2.5 %
1.5 - 2.5 %
Nickel, Ni >= 97 %
>= 97 %
Including Cobalt
Silicon, Si <= 0.20 %
<= 0.20 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000109 ohm-cm