Spartech Sound X Noise Abatement Alloy Specialty Sheet

Category Polymer , Thermoplastic
Manufacturer Spartech
Trade Name Sound X
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Sound X Noise Abatement Alloy Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 2.00 g/cc
2.00 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Yield Strength 44.8 MPa
6500 psi
ASTM D790