Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet

Category Polymer , Thermoplastic , ABS Polymer , ASA Polymer
Manufacturer Spartech
Trade Name Soft Touch
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Soft Touch ASA/ABS Co-Extruded Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Unnotched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648