Spartech Royalstatâ„¢ R671 ABS Static Control Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Royalstatâ„¢ R671 ABS Static Control Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
Tensile Strength, Ultimate 27.6 MPa
4000 psi
Machine direction
Flexural Yield Strength 45.5 MPa
6600 psi
Flexural Modulus 1.70 GPa
247 ksi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Electrical Properties Metric English Comments
Surface Resistance <= 1e+05
<= 1e+05