Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Royalstatâ„¢ R63 ABS/PVC Static Control Sheet

Category Polymer , Thermoplastic , ABS Polymer , ABS/PVC Alloy , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Royalstatâ„¢ R63 ABS/PVC Static Control Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Static Control SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Flexural Yield Strength 49.0 MPa
7100 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Falling Dart Impact 217 J

@Temperature -40.0 °C
160 ft-lb

@Temperature -40.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C
165 °F
ASTM D648
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1e+05
<= 1e+05
ASTM D257