Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Spartech
Trade Name Polypro
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Polypro SP-1710 Co/Pol Polyolefin Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyolefin SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
ASTM D2240
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 20.0 °C
60.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: