Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech PolyTeak Low Stress HDPE Specialty Sheet

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Manufacturer Spartech
Trade Name PolyTeak
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech PolyTeak Low Stress HDPE Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Tensile Modulus 0.655 GPa
95.0 ksi
ASTM D638
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Unnotched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 108 µm/m-°C

@Temperature 20.0 °C
60.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Users viewing this material also viewed the following: