Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name Panel Pro
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Panel Pro ABS UV-Resistant Embossed Sheet Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Unnotched 4.00 J/cm
7.50 ft-lb/in
ASTM D256
1.33 J/cm

@Temperature -40.0 °C
2.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 92.2 °C
198 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 86 %
86 %
Gardner; ASTM D2523
Descriptive Properties Value Comments
Flammability Passes
MVSS (Motor Vehicle Safety Standard) 302
Users viewing this material also viewed the following: