Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech PP5440 Glass Fiber Reinforced Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech PP5440 Glass Fiber Reinforced Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc

@Temperature 22.8 °C
1.23 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 40 %
40 %
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 89.6 MPa
13000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Elongation at Yield 1.0 %
1.0 %
ASTM D638
Flexural Strength 131 MPa
19000 psi
Max Load; ASTM D790
Flexural Modulus 5.52 GPa
800 ksi
secant; ASTM D790
7.58 GPa
1100 ksi
tangent; ASTM D790
Izod Impact, Notched 0.854 J/cm

@Temperature 22.8 °C
1.60 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM D648