Spartech Noryl® GTX SP-52Z1 Structural Sheet

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer Spartech
Trade Name Noryl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Noryl® GTX SP-52Z1 Structural Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Structural SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 83 %
83 %
ASTM D638
Flexural Yield Strength 95.8 MPa
13900 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Unnotched 3.36 J/cm
6.30 ft-lb/in
ASTM D256
1.23 J/cm

@Temperature -28.9 °C
2.30 ft-lb/in

@Temperature -20.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 179 °C
355 °F
ASTM D648