Spartech MG6024GP PVC and Alloy Products for Footwear

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech MG6024GP PVC and Alloy Products for Footwear.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used for economical soling/ bottoming. Comes only in black.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60