Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech Formalloy TPR Thermoplastic Rubber Alloy Specialty Sheet

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Spartech
Trade Name Formalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Formalloy TPR Thermoplastic Rubber Alloy Specialty Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Specialty SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell L 88
88
ASTM D785
Tensile Strength at Break 7.770 MPa
1127 psi
ASTM D638
Elongation at Break 627 %
627 %
ASTM D638
Flexural Modulus 0.1190 GPa
17.26 ksi
ASTM D790
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Optical Properties Metric English Comments
Gloss 20 - 25 %
20 - 25 %
Gardner; ASTM D2523