Spartech DKE® 450 450 PVC/Acrylic Fire Rated Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech DKE® 450 450 PVC/Acrylic Fire Rated Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
Tensile Strength, Ultimate 46.9 MPa
6800 psi
Machine direction
Flexural Yield Strength 75.8 MPa
11000 psi
Flexural Modulus 2.60 GPa
377 ksi
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
0.500 J/cm

@Temperature -29.0 °C
0.937 ft-lb/in

@Temperature -20.2 °F
Gardner Impact >= 27.0 J
>= 19.9 ft-lb
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
Flammability, UL94 V-0
V-0