Spartech Centrex® R83/21 ABS Weather Resistant Sheet

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Sheet
Manufacturer Spartech
Trade Name Centrex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Centrex® R83/21 ABS Weather Resistant Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Machine direction
Flexural Yield Strength 55.2 MPa
8010 psi
Flexural Modulus 1.90 GPa
276 ksi
Izod Impact, Notched 3.70 J/cm
6.93 ft-lb/in
1.10 J/cm

@Temperature -29.0 °C
2.06 ft-lb/in

@Temperature -20.2 °F
Gardner Impact >= 32.0 J
>= 23.6 ft-lb
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F