Spartech 2850-70 PVC for Regulated Applications

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech 2850-70 PVC for Regulated Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 14.5 MPa
2100 psi
Elongation at Break 410 %
410 %
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F