Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: Due to its outstanding flow characteristics, the product provides a significant productivity improvement and allows more freedom in mould and part design versus a standard polyamide solutions.Available in: Asia Pacific, Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: It is used in a wide variety of industries.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527 Type 1A
Elongation at Break 4.5 %
4.5 %
ISO 527 Type 1A
Tensile Modulus 6.20 GPa
899 ksi
ISO 527 Type 1A
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 4.75 GPa
689 ksi
ASTM D790
4.90 GPa
711 ksi
ISO 178
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 3.15 J/cm²
15.0 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %