Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, Conditioned

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYL® R
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® R AR 130/GF Nylon 66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® AR 130/GF is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color. Benefits: The product offers a good combination between thermal and mechanical properties.Available in: Europe Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC This grade complies with RoHS directive 2002/95/EC Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: It is used in a wide variety of industries for applications without severe impact resistance requirements, such as fans and shrouds components in automotive.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ISO 527 Type 1A
Tensile Modulus 6.00 GPa
870 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %