Solvay TECHNYL® C 538XT V30 Natural W PA6, 30% glass filled, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 538XT V30 Natural W PA6, 30% glass filled, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 6 reinforced with 30% of glass fibers, heat stabilized, with high viscosity and high toughness, for extrusion.Available in: North America Product Applications: This product is designed specifically for extrusion to be used in window profile and thermal break applications. This material is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Mechanical Properties Metric English Comments
Tensile Strength at Break 142 MPa
20600 psi
ISO 527 Type 1A
Elongation at Break 142 %
142 %
ISO 527 Type 1A
Tensile Modulus 8.90 GPa
1290 ksi
ISO 527 Type 1A
Flexural Strength 221 MPa
32100 psi
ISO 178
Flexural Modulus 6.626 GPa
961.0 ksi
ISO 178
Izod Impact, Notched (ISO) 24.98 kJ/m²
11.89 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.28 J/cm²
44.2 ft-lb/in²
ISO 179/1eU
Processing Properties Metric English Comments
Feed Temperature 240 - 260 °C
464 - 500 °F
Front Barrel Temperature 240 - 280 °C
464 - 536 °F
Descriptive Properties Value Comments
Compression Zone 240-270°C