Solvay TECHNYL® C 536XT PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 536XT PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing behavior, high impact resistance even at low temperature and high barrier properties especially to fluids such as fuels and oils, as well as a high toughness.Available in: Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: This grade is particularly recommended for use in applications such as tanks or pipes.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
ISO 527 Type 1A
Elongation at Break 190 %
190 %
ISO 527 Type 1A
Tensile Modulus 0.910 GPa
132 ksi
ISO 527 Type 1A
Flexural Modulus 0.650 GPa
94.3 ksi
ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.080 %
<= 0.080 %