Solvay TECHNYL® C 502XT PA6, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 502XT PA6, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced polyamide 6, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rods, profiles, sheets, pipes. All the semi-finished products can be machined without special treatment, such as: Precision gears, bolts, etc. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183/A
Water Absorption 1.37 %

@Temperature 23.0 °C,
Time 86400 sec
1.37 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527 type 1 A
Elongation at Break 160 %
160 %
ISO 527 Type 1A
Elongation at Yield 4.2 %
4.2 %
ISO 527 type 1 A
Tensile Modulus 2.80 GPa
406 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.4
3.4
IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Dissipation Factor 0.020
0.020
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 230 °C
446 °F
Front Barrel Temperature 230 °C
446 °F
Die Temperature 240 °C
464 °F
Descriptive Properties Value Comments
Compression Zone 230ºC