Solvay TECHNYL® C 402 M PA6, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 402 M PA6, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high flexibility and high impact strength. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Water Absorption 1.9 %

@Temperature 23.0 °C,
Time 86400 sec
1.9 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527 type 1 A
Tensile Modulus 1.20 GPa
174 ksi
ISO 527 Type 1A
Flexural Strength 50.0 MPa
7250 psi
ISO 178
Flexural Modulus 1.00 GPa
145 ksi
ISO 178
Izod Impact, Notched (ISO) 14.5 kJ/m²
6.90 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.6
3.6
IEC 60250
Dissipation Factor 0.020
0.020
IEC 60250
Processing Properties Metric English Comments
Feed Temperature 225 - 230 °C
437 - 446 °F
Front Barrel Temperature 235 - 245 °C
455 - 473 °F
Mold Temperature 40.0 °C
104 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 230-240°C