Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 50

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stability, Impact resistance and Stiffness Applications: TECHNYL C 218 V15 was developed for applications on parts where good mechanical properties as impact resistance, superficial aspect and dimensional stability are required.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ISO R 527
Elongation at Break 7.0 %
7.0 %
Rupture; ISO R 527
Tensile Modulus 2.90 GPa
421 ksi
ISO R 527
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 5.80 J/cm²
27.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
CEI 93
Dielectric Constant 4.5
4.5
CEI 250
Dielectric Strength 22.0 kV/mm
559 kV/in
CEI 93
Dissipation Factor 0.090
0.090
CEI 250
Comparative Tracking Index 475 V
475 V
CEI 112