Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® C 206 PA6, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 206 PA6, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored by a high crystallization rate. It is especially suitable for the production of technical moldings with fast injection cycles. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Water Absorption 1.3 %

@Temperature 23.0 °C,
Time 86400 sec
1.3 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.0 MPa
12300 psi
ISO 527 type 1 A
Tensile Modulus 2.85 GPa
413 ksi
ISO 527 Type 1A
Flexural Strength 115 MPa
16700 psi
ISO 178
Flexural Modulus 2.80 GPa
406 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75/Af
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.4
3.4
IEC 60250
Dissipation Factor 0.020
0.020
IEC 60250
Processing Properties Metric English Comments
Feed Temperature 220 - 230 °C
428 - 446 °F
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Mold Temperature 20.0 - 50.0 °C
68.0 - 122 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 225-235°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved