Material Notes:
Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: The product offers an excellent long term heat resistance and is suitable to work in environments characterized by a very high temperature.Available in: EuropeRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: Thanks to its high melt strength, this product can be used to produce hollow parts, by suction blow molding technology, like tanks or ducts. Typical applications are turbo air ducts, especially inlet ducts up to 200°C.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527 Type 1A
Elongation at Break 9.0 %
9.0 %
ISO 527 Type 1A
Tensile Modulus 3.50 GPa
508 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.080 %
<= 0.080 %