Material Notes:
Description: Flame retardant polyamide PA66, 40% mineral filled, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This flame retardant material offers very good dimensional stability and excellent Glow wire performance. This product is particularly recommended for electrical parts such as: low voltage distribution, protection systems, mini circuit breakers, fuse holders and terminal blocks. This product is available in grey.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ISO 1183/A
Water Absorption 0.43 %

@Temperature 23.0 °C,
Time 86400 sec
0.43 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 77.0 MPa
11200 psi
ISO 527 Type 1A
Elongation at Break 1.7 %
1.7 %
ISO 527 Type 1A
Tensile Modulus 6.90 GPa
1000 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.220 J/cm²
1.05 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ISO 75/Af
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
1210
Oxygen Index 46.5 %
46.5 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 0.800 mm
1760 °F

@Thickness 0.0315 in
ISO 60695-2-12
960 °C

@Thickness 1.60 mm
1760 °F

@Thickness 0.0630 in
ISO 60695-2-12
960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
ISO 60695-2-12
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Comparative Tracking Index 400 V
400 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 270 - 275 °C
518 - 527 °F
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 285-290°C