Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This flame retardant material, U.L. 94 V0 rated at 0.8 mm, shows high Glow-wire, CTI values and good mechanical properties .It can be supplied in various colors. This grade is suitable for molding insulating parts for electrical devices: switches, rotary switches, timers and contactors. This product is available in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.0 MPa
11300 psi
ISO 527 Type 1A
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 4.70 J/cm²
22.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Copyright © lookpolymers.com All Rights Reserved