Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 238 Black 21 N PA66, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 238 Black 21 N PA66, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent combination between rigidity and impact resistance at ambient temperature. This property save special conditioning before use parts (water absorption). This grade is commonly used for under bonnet automobile parts , such as: fasteners, cable ties. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183/A
Water Absorption 1.1 %

@Temperature 23.0 °C,
Time 86400 sec
1.1 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Linear Mold Shrinkage, Transverse 0.019 cm/cm
0.019 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527 Type 1A
Tensile Strength, Yield 70.0 MPa
10200 psi
ISO 527 type 1 A
Elongation at Break 30 %
30 %
ISO 527 Type 1A
Elongation at Yield 5.0 %
5.0 %
ISO 527 type 1 A
Tensile Modulus 2.55 GPa
370 ksi
ISO 527 Type 1A
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.25 GPa
326 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C
505 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Oxygen Index 21 %
21 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.2
3.2
IEC 60250
Dielectric Strength 32.0 kV/mm
813 kV/in
IEC 60243
Dissipation Factor 0.020
0.020
IEC 60250
Comparative Tracking Index 450 V
450 V
Solution B; IEC 60112
500 V
500 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 240 - 250 °C
464 - 482 °F
Front Barrel Temperature 260 - 270 °C
500 - 518 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 250-260°C
Copyright © lookpolymers.com All Rights Reserved