Solvay TECHNYL® A 222 Black 1N PA66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 222 Black 1N PA66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity .These performances are associated with excellent dimensional stability and good rigidity of molded parts. This grade is used for connector parts in electrical and automotive industries. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527 Type 1A
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527 type 1 A
Elongation at Break 105 %
105 %
ISO 527 Type 1A
Elongation at Yield 25 %
25 %
ISO 527 type 1 A
Tensile Modulus 2.00 GPa
290 ksi
ISO 527 Type 1A
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 3.2
3.2
IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Dissipation Factor 0.080
0.080
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %