Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phosphorus flame retardant grade, offers excellent filling qualities and with good mechanical properties. This grade is stabilized to offer a very low migration and corrosion of metallic contacts. It is particularly suitable for molding insulating parts for electrical devices: connectors, contactors, bobbins coil formers and thin parts under stress. This product is available in natural and black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183/A
Water Absorption 0.90 %

@Temperature 23.0 °C,
Time 86400 sec
0.90 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527 Type 1A
Elongation at Break 2.7 %
2.7 %
ISO 527 Type 1A
Tensile Modulus 8.70 GPa
1260 ksi
ISO 527 Type 1A
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 7.90 GPa
1150 ksi
ISO 178
Charpy Impact Unnotched 6.10 J/cm²
29.0 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
ISO 75/Af
Flammability, UL94 V-2

@Thickness 0.800 mm
V-2

@Thickness 0.0315 in
1210
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
1210
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
1210
Oxygen Index 28 %
28 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 0.800 mm
1760 °F

@Thickness 0.0315 in
ISO 60695-2-12
960 °C

@Thickness 1.60 mm
1760 °F

@Thickness 0.0630 in
ISO 60695-2-12
960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
ISO 60695-2-12
Electrical Properties Metric English Comments
Comparative Tracking Index 500 V
500 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C