Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature. The product offers an improved hydrolisis resistance, as well as an excellent combination between thermal and mechanical properties. It also restricts electrolytical corrosion.Available in: Asia Pacific and EuropeRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water, such as electro-magnetic valves. It can also be used as insulation material for electronic connectors, due to its limited electrolytical corrosion.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183/A
Water Absorption 0.80 %

@Temperature 23.0 °C,
Time 86400 sec
0.80 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity 120 cP

@Shear Rate 100 1/s,
Temperature 290 °C
120 cP

@Shear Rate 100 1/s,
Temperature 554 °F
150 cP

@Shear Rate 100 1/s,
Temperature 280 °C
150 cP

@Shear Rate 100 1/s,
Temperature 536 °F
200 cP

@Shear Rate 100 1/s,
Temperature 270 °C
200 cP

@Shear Rate 100 1/s,
Temperature 518 °F
205 cP

@Shear Rate 10.0 1/s,
Temperature 290 °C
205 cP

@Shear Rate 10.0 1/s,
Temperature 554 °F
300 cP

@Shear Rate 10.0 1/s,
Temperature 280 °C
300 cP

@Shear Rate 10.0 1/s,
Temperature 536 °F
500 cP

@Shear Rate 10.0 1/s,
Temperature 270 °C
500 cP

@Shear Rate 10.0 1/s,
Temperature 518 °F
Linear Mold Shrinkage 0.0062 cm/cm
0.0062 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 190 MPa
27600 psi
ISO 527 Type 1A
Tensile Stress 85.0 MPa

@Strain 1.00 %
12300 psi

@Strain 1.00 %
155 MPa

@Strain 2.00 %
22500 psi

@Strain 2.00 %
180 MPa

@Strain 3.00 %
26100 psi

@Strain 3.00 %
Elongation at Break 3.2 %
3.2 %
ISO 527 Type 1A
Tensile Modulus 1.00 GPa
145 ksi
ISO 527 Type 1A
Flexural Strength 270 MPa
39200 psi
ISO 178
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
9.00 GPa
1310 ksi
ISO 178
Izod Impact, Notched 1.05 J/cm
1.97 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 28.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
15.6 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
CTE, linear, Transverse to Flow 2.80 µm/m-°C

@Temperature 23.0 - 85.0 °C
1.56 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 262 °C
504 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM D648
254 °C
489 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Glow Wire Test 700 °C

@Thickness 1.60 mm
1290 °F

@Thickness 0.0630 in
ISO 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 3.7
3.7
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243
Dissipation Factor 0.020
0.020
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 265 - 275 °C
509 - 527 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C