Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218W V15 PA66, 15% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, reinforced with 15% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: North AmericaProduct Applications: TECHNYL ® a 218W V15 is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is recommended for the production of mechanical components in permanent or intermittent contact with hot water: e.g. electro-magnetic valves. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183/A
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %