Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature.Available in: Asia Pacific, Europe and Latin AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: It is used in a wide variety of industries, especially in automotive industry for air circuit parts such as intercoolers.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 143 MPa
20700 psi
ISO 527 Type 1A
Elongation at Break 2.0 %
2.0 %
ISO 527 Type 1A
Tensile Modulus 10.5 GPa
1520 ksi
ISO 527 Type 1A
Flexural Strength 230 MPa
33400 psi
ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Charpy Impact Unnotched 9.40 J/cm²
44.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.30 J/cm²
10.9 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.12 %
<= 0.12 %