Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 218HP V30 BLACK 21N offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature. Offering an excellent combination between thermal and mechanical properties, it is used in all sectors of industry, such as in the automotive for engine components and in the electrical field for bobbin coil.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527 Type 1A
Elongation at Break 5.5 %
5.5 %
ISO 527 Type 1A
Tensile Modulus 6.60 GPa
957 ksi
ISO 527 Type 1A
Flexural Strength 180 MPa
26100 psi
ISO 178
Flexural Modulus 5.90 GPa
856 ksi
ISO 178
Charpy Impact Unnotched 7.70 J/cm²
36.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.12 %
<= 0.12 %