Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry for engine components. This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
ISO 527 Type 1A
Tensile Strength, Yield 165 MPa
23900 psi
ISO 527 type 1 A
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 9.40 GPa
1360 ksi
ISO 527 Type 1A
Flexural Modulus 7.80 GPa
1130 ksi
ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²
9.04 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 450 V
450 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Copyright © lookpolymers.com All Rights Reserved