Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: This product has enhanced molding behaviors and better surface aspect. It offers an excellent combination between thermal and mechanical properties. This grade is ideal for use in the automotive industry for engine components. This grade is ideal for Mucell® injection molding technology.Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: This grade is suitable for all kind of applications in automotive (pulleys, Inlet manifolds, air-ducts, engine covers) and non automotive that required a good balanced behavior between surface aspect, thermal and mechanical behavior.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Water Absorption 0.75 %

@Temperature 23.0 °C,
Time 86400 sec
0.75 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity 130 cP

@Shear Rate 100 1/s,
Temperature 275 °C
130 cP

@Shear Rate 100 1/s,
Temperature 527 °F
300 cP

@Shear Rate 10.0 1/s,
Temperature 275 °C
300 cP

@Shear Rate 10.0 1/s,
Temperature 527 °F
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0045 cm/cm
0.0045 in/in
Linear Mold Shrinkage, Transverse 0.0075 cm/cm
0.0075 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
ISO 527 Type 1A
Tensile Stress 110 MPa

@Strain 1.00 %
16000 psi

@Strain 1.00 %
180 MPa

@Strain 2.00 %
26100 psi

@Strain 2.00 %
205 MPa

@Strain 3.00 %
29700 psi

@Strain 3.00 %
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 11.1 GPa
1610 ksi
ISO 527 Type 1A
Flexural Strength 280 MPa
40600 psi
ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75/Af
Processing Properties Metric English Comments
Feed Temperature 265 - 275 °C
509 - 527 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C