Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The product offers an excellent combination between thermal and mechanical properties.Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications. Applications: It is used in a wide variety of industries.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Flexural Strength 185 MPa
26800 psi
ISO 178
Flexural Modulus 6.40 GPa
928 ksi
ISO 178
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved