Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V25 BLACK 21NHFE is characterized by a high flowability and offers an excellent combination between thermal and mechanical properties. This grade is a perfect fit for the pulley application and gives very low rugosity levels. This grade improves the surface aspect and reduce the warpage of the parts. In the automotive industry, this Technyl grade definitely meets the requirements for engine components, such as: inlet manifold, air ducts - engine covers, pulleys and various housings and liquid containers. This product is available in blackInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183/A
Water Absorption 0.90 %

@Temperature 23.0 °C,
Time 86400 sec
0.90 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0071 cm/cm
0.0071 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0085 cm/cm
0.0085 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527 Type 1A
Elongation at Break 2.7 %
2.7 %
ISO 527 Type 1A
Tensile Modulus 8.80 GPa
1280 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 5.50 J/cm²
26.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75/Af
Processing Properties Metric English Comments
Feed Temperature 270 - 275 °C
518 - 527 °F
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 280-285°C