Material Notes:
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry and electrical sectors. This product is available in natural and black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ISO 527 Type 1A
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527 type 1 A
Elongation at Break 8.0 %
8.0 %
ISO 527 Type 1A
Tensile Modulus 4.30 GPa
624 ksi
ISO 527 Type 1A
Flexural Strength 11.5 MPa
1670 psi
ISO 178
Flexural Modulus 3.50 GPa
508 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 6.70 J/cm²
31.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 325 V
325 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %