Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 S40 Black 21 N PA66, 40% glass spheres, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, reinforced with 40% of glass spheres, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL ® A 218 S40 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is recommended for mechanical components which require a very good surface finish with low warpage, and good compression strength (bearing housings). This product is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527 Type 1A
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527 type 1 A
Elongation at Break 35 %
35 %
ISO 527 Type 1A
Elongation at Yield 20 %
20 %
ISO 527 type 1 A
Tensile Modulus 3.00 GPa
435 ksi
ISO 527 Type 1A
Flexural Strength 75.0 MPa
10900 psi
ISO 178
Flexural Modulus 2.45 GPa
355 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 5.00e+10 ohm
5.00e+10 ohm
IEC 60093
Dielectric Constant 5.0
5.0
IEC 60250
Dielectric Strength 26.0 kV/mm
660 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 400 V
400 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %