Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is suitable for automotive industry. This material is available in black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 8.30 GPa
1200 ksi
ISO 527 Type 1A
Flexural Modulus 6.40 GPa
928 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 9.80 J/cm²
46.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %