Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offering and excellent combination between thermal and mechanical properties. This grade is used in: automotive industry, manufacture of components for electrical tools, and transport and building. This product is available in natural, grey and black and in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ISO 527 Type 1A
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527 type 1 A
Elongation at Break 8.0 %
8.0 %
ISO 527 Type 1A
Tensile Modulus 4.30 GPa
624 ksi
ISO 527 Type 1A
Flexural Modulus 3.50 GPa
508 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 6.70 J/cm²
31.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²
3.57 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %