Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This phosphorus and halogen free flame retardant grade is particularly suitable for equipment with robust glow wire resistance such as MCB housings. This grade is available in grey color.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 4.00 GPa
580 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %