Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excellent combination between the mechanical properties. This grade is used for It is used in the automotive industry and electrical sectors. Door motor cover. This product is available in Natural, black, gray and in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Water Absorption 0.95 %

@Temperature 23.0 °C,
Time 86400 sec
0.95 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.000035 cm/cm
0.000035 in/in
Linear Mold Shrinkage, Transverse 0.0065 cm/cm
0.0065 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D786
Tensile Strength, Yield 175 MPa
25400 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 260 MPa
37700 psi
ASTM D790
Flexural Modulus 8.90 GPa
1290 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D265
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Flammability, UL94 HB
HB
ISO 1210
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
IEC-60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dissipation Factor 0.020
0.020
IEC 60250
Comparative Tracking Index 550 V
550 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 230 - 235 °C
446 - 455 °F
Front Barrel Temperature 245 - 250 °C
473 - 482 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 235-345°C
Copyright © lookpolymers.com All Rights Reserved