Solvay Specialty Polymers Tecnoflon® N 935 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Tecnoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Tecnoflon® N 935 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tecnoflon® N 935 is a medium high viscosity fluoroelastomer copolymer. Tecnoflon® N 935 is intended as a general purpose fluoroelastomer. It can be blended with other polymers of the Tecnoflon® family to meet specific requirements. Tecnoflon® N 935 does not contain curatives: therefore the proper levels of Tecnoflon® FOR M1 and Tecnoflon® FOR M2 must be added to achieve the required properties. It can be also cured with diamine based systems such as Tecnoflon® Tecnocin A and Tecnoflon® Tecnocin B.Features: Copolymer; General Purpose; Good Flow; Good Mold Release; Low Compression Set; Medium-high ViscosityUses: Belts/Belt Repair; Blending; Gaskets; General Purpose; Hose; Profiles; Seals; SheetAdditional Properties: Fluorine Content - 66 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Mooney Viscosity 62

@Temperature 121 °C
62

@Temperature 250 °F
ML 1+10; ASTM D1646
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.2600
Availability Europe; North America
Color Translucent
Form Slab
Processing Technique Calendering; Compounding; Compression Molding; Extrusion