Solvay Specialty Polymers Tecnoflon® FOR 5381 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Tecnoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Tecnoflon® FOR 5381 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECNOFLON® FOR 5381 is a low viscosity cure incorporated fluoroelastomer terpolymer (FKM) with 68.5% fluorine content. Tecnoflon® FOR 5381 is well suited for all applications requiring better chemical resistance and/or long term heat resistance compared to fluoroelastomer copolymers. Tecnoflon® FOR 5381 contains proprietary cure system and special process aid providing superior processability for fast cycles and scorch safety.Features: Fast Molding Cycle; Good Chemical Resistance; Good Heat Aging Resistance; Good Processability; High Heat Resistance; Low Compression Set; Low Viscosity; TerpolymerUses: Belts/Belt Repair; Blending; Gaskets; Hose; Profiles; Seals; Sheet; Valves/Valve PartsAdditional Properties: Fluorine Content - 69 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Mooney Viscosity 21

@Temperature 121 °C
21

@Temperature 250 °F
ML 1+10; ASTM D1646
Descriptive Properties Value Comments
Additive Processing Aid
Availability Europe; North America
Color Off-White
Form Slab
Processing Technique Calendering; Compounding
Compression Molding; Extrusion
Injection Molding; Resin Transfer Molding