Solvay Specialty Polymers Polymist® F5A EX Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Polymist®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® F5A EX Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® F5A EX is a white PTFE micronized powder PTFE micronized powder composed of discrete particles. Designed for use in critical engineering and high end performance plastics applications, Polymist® F5A EX will improve wear resistance and reduce coefficient of friction.Uses: AdditiveAdditional Properties: Average Particle Size - Internal Method 12 µm; Bulk Density - ASTM D4895 500 g/l; Melt Temperature - ASTM D3418 325 to 335 °C; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder