Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Polymist® F284 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Polymist®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® F284 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® F284 is a white micronized PTFE powder composed of discrete particles. Available worldwide, Polymist® F284 is a medium molecular weight grade with excellent thermal stability, designed for use in critical high temperature engineering and high performance polymers. As with all Polymist® micronized powders, F284 offers excellent chemical and temperature residence, low surface energy, low coefficient of friction and good dispersion ability.Uses: AdditiveAdditional Properties: Average Particle Size - Internal Method 9.0 µm; Bulk Density - ASTM D4895 400 g/l; Grind in Oil - NPIRI 5.00; Melt Temperature - ASTM D3418 325 to 335 °C; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder